①High print head temperature will lead to easy outflow of filaments.Reduce the print head temperature of 5-10 ℃, increase the pullback distance and speed, and reduce the printing speed.
②If you print multiple models at the same time, increase the idle driving speed and reduce the distance between models.
The print head may be slightly blocked. Click to preheat PLA and use a steel needle to dredge the print head nozzle. Or replace a spare print head test.
If you have further questions, we suggest you create an after-sales ticket and our After-sales engineers will help you solve the problem. (Reply time :1 working day)