Since this page is the content of the general -purpose sector, we will provide solutions on this page, but we cannot provide specific operation steps for each device.
The model that has been solidified appears in the resin vat.
Our suggestions are:
The reason is that the normal exposure time is relatively short, resulting in the resin is not completely solidified.
Our suggestions are:
Increase the exposure time layer by 30%,
The model does not have Post-Cure. It is recommended to clean the model, air dry, and solidify the ultraviolet offline.
It may be because the liquid resin has some solidified debris.
Our suggestions are:
This situation will occur in insufficient air pressure in the hollow model.
We suggest that if you operate Hollow and operate the PUNCH together to ensure that the inner and outer pressure of the model is consistent.
Other problems, we feel that it may not have a relationship with the resin, so we put on another page, please click on the link below to jump.